Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® 2258 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® 2258 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
  • MVR (300 °C/1.2 kg) 34 cm³/10 min
  • medical devices
  • suitable for ETO and steam sterilization at 121 °C
  • biocompatible according to many ISO 10993-1 test requirements
  • low viscosity
  • easy release
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 34 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Índice de fluidez, MFI 37 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.7 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2400 MPa ISO 527
Esfuerzo de fluencia 65 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Módulo de flexión, 23°C 2350 MPa ISO 178
Resistencia a la flexión 97 MPa ISO 178
Módulo de plastodeformación, 1h 2100 MPa ISO 899-1
Módulo de plastodeformación, 1000h 1700 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 55 kJ/m² ISO 179/1eA
Type of failure P(C) - -
Resistencia al impacto Charpy c/entalla, -30°C 12 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Izod con entalla, +23°C 55 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 12 kJ/m² ISO 180/1A
Temperatura -30 °C -
Perforación - máxima fuerza, +23°C 4900 N ISO 6603-2
Perforación - máxima fuerza, -30°C 5900 N ISO 6603-2
Perforación - energía, +23°C 55 J ISO 6603-2
Perforación - energía, -30°C 60 J ISO 6603-2
Ball indentation hardness 115 MPa ISO 2039-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. de transición vítrea, 10°C/min 145 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 124 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 137 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 145 °C ISO 306
Coef.de expansión térmica lineal, paralelo 65 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 65 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Yellow Card disponible - -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 900 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Other Standards[S]
Conductividad térmica, estado sólido 0.2 W/(m K) ISO 8302
S: These properties are reported by the producer according standards that are different to our defaults.
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.1 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 5 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 90 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 34 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 250 - IEC 60112
Propiedades opticasValorUnidadesMétodo de ensayo
ISO Data
Niebla 0.8 - ISO 14782
Transmitancia luminosa 89 % ISO 13468-1, -2
Other Standards[S]
Índice de refracción 1.59 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.3 % Sim. to ISO 62
Absorción de humedad 0.12 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Bulk density 660 kg/m³ -
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 280 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 2 - 3 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 280 - 320 °C -
Temperatura del molde 80 - 120 °C -
Zona 1 250 - 260 °C -
Zona 2 270 - 280 °C -
Zona 3 280 - 290 °C -
Temperatura de boquilla 290 - 300 °C -
Contrapresión 5 - 15 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Desmoldeante
Características especiales
Transparente, Opaque, Esterilizable, Esterilización por óxido de etileno (EtO), Esterilización por vapor
Certifications
Contiene recursos renovables, Grado médico, Biocompatibility ISO 10993, ISCC Plus
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.