![Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.](/rev13959/modules/../customized/tradenames/views/images/seo_en.png)
Material datasheets available free. Online registration at: www.materialdatacenter.com
Microthene - EVAC, PE-HD, PE-LD, PE-LLD - LyondellBasell Industries
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Microthene" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
Microthene MN72700 | (PE-LD) |
Microthene FA70000 | (PE-HD) |
Microthene FA70900 | (PE-HD) |
Microthene FE53200 | EVAC |
Microthene FN50100 | (PE-LD) |
Microthene FN51000 | (PE-LD) |
Microthene FN51900 | (PE-LD) |
Microthene MN70100 | (PE-LD) |
Microthene MN71020 | (PE-LD) |
Microthene MN71120 | (PE-LD) |
Microthene MN71400 | (PE-LD) |
Microthene MN72200 | (PE-LD) |
Microthene MP564189 | (PE-LLD) |
Microthene MP574189 | (PE-LLD) |
Microthene MP625962 | (PE-LLD) |
Microthene MP635962 | (PE-LLD) |
Microthene MP643962 | (PE-LLD) |
Microthene MP652962 | (PE-HD) |
Microthene MP672962 | (PE-HD) |
Microthene MU76000 | EVAC |
Microthene MU76300 | EVAC |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.