Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of P84®UHT 15G HCM - PI-CD - Evonik Operations GmbH

Material Data Center offers the following functions for P84®UHT 15G HCM:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other P84 datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

High temperature resistance, graphite filled (15%) Polyimide

Polyimid P84®UHT - at a glance

 

  • Excellent thermal-oxidative stability (use up to 300 ° C)
  • High mechanical strength and dimensional stability even at very high temperatures
  • Good creep resistance under load even at high temperatures
  • Easy machinability with standard tools for metals
  • Excellent tribological properties, high wear resistance
  • Processing by hot compression molding

 

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

For further information please visit WWW.P84.COM.

Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 7030 MPa ISO 527
Resistencia a la tracción 106 MPa ISO 527
Alargamiento a rotura 2.3 % ISO 527
Resistencia al impacto Charpy, +23°C 28 kJ/m² ISO 179/1eU
Type of failure C - -
Resistencia al impacto Charpy c/entalla, +23°C 2 kJ/m² ISO 179/1eA
Type of failure C - -
Dureza Shore D 86 - ISO 7619-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 272 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 318 °C ISO 75-1/-2
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1510 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por compresión
Forma de suministro
Sémola, Granulado, Polvo
Aditivos
Lubricante
Características especiales
Estable contra el calor
Características
Resistencia a la fluencia, Estabilidad térmica, Grado tribológico
Resistencia quimica
Resistencia a la oxidación
Applicaciones
Avión y aeroespacial, Automotriz
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com