Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 3533 SA 01 MED - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 3533 SA 01 MED:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Polyether block amide Pebax® 3533 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.
Upon request, letters regarding USP Class VI compliance can be provided.


Main applications:
  • Catheters
  • Flexible injected parts


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 19 / 18 MPa ISO 527
Esfuerzo a 50% de alarg. 4 / 4 MPa ISO 527
Alargamiento a rotura >50 / >50 % ISO 527
Resistencia a la tracción TPE 39 / * MPa ISO 527
Alargamiento a rotura TPE >300 / * % ISO 527
Dureza Shore A 80 / * - ISO 7619-1
Dureza Shore D 25 / * - ISO 7619-1
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 144 / * °C ISO 11357-1/-3
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.2 / * % Sim. to ISO 62
Absorción de humedad 0.4 / * % Sim. to ISO 62
Densidad 1000 / 1000 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 55 - 65 °C -
Tiempo de pre-secado 4 - 8 h -
Temperatura de la masa 180 - 240 °C -
Temperatura del molde 10 - 30 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Otros tipos de extrusión
Forma de suministro
Sémola
Aditivos
Lubricante
Características especiales
Estable contra el calor
Certifications
Grado médico, USP Class VI
Disponibilidad regional
Demás información
Moldeo por inyección

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 180°C / 210°C / 240°C.
- Typical mold temperature : 10 – 30°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.
Otros tipos de extrusión

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 190°C / 205°C / 220°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.