Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® M 1276 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® M 1276 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Platamid® M 1276 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 1276 is a thermoplastic co-polyamide hot melt adhesive available in pellet form. This medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.

Platamid®  M 1276 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc). 

In addition, Platamid®  M 1276 also exhibits strong adhesion onto rigid and plasticized PVC as well as ABS, epoxy resin, PU etc.

Dense layers of Platamid®  M 1276 are known to have barrier properties against PVC plasticizer migration.

According to ASTM D6866, the biobased carbon content is measured at 26%.




AVAILABLE GRADES
This product is available:
- Dried (M 1276 TE)
- Un-dried (M 1276 F)
PACKAGING
- Platamid® M 1276 TE is delivered in 25 kg sealed bags.
- Platamid®M 1276 F is delivered in 25 kg sealed bags and 500 kg sealed big bags (GRVS).
These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
RENEWABLE CARBON
26% (according ASTM D6866)
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 6 / * cm³/10min ISO 1133
Temperatura 160 / * °C -
Carga 2.16 / * kg -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 110 / * °C ISO 11357-1/-3
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1100 / 1100 kg/m³ ISO 1183
Biobased content 26 % -
Características
Procesamiento y forma de entrega
Extrusion del film
Forma de suministro
Sémola
Características
Propiedades de barrera, Buenas propiedades de adhesión, Copolímero
Certifications
Contiene recursos renovables
Applicaciones
Monofilamento, Filamentos multiple
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.