Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Plenco 04309 - PF-GF - Plastics Engineering Co.

Material Data Center offers the following functions for Plenco 04309:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Plenco datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.0067 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 9331 MPa ASTM D 638
Esfuerzo de tracción 48 MPa ASTM D 638
Resistencia de compresión 165 MPa ASTM D 695
Módulo de flexión 8617 MPa ASTM D 790
Resistencia a la flexión 80.4 MPa ASTM D 790
Dureza Rockwell E 80 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 20.9 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 V-0 - UL 94
Espesores de probeta 1.5 mm -
Estabilidad al calor @ 264 psi 164 °C ASTM D 648
Índice de oxigeno límite 30.6 % ASTM D 2863
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia dieléctrica, tiempo corto 7.9 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.06 - ASTM D 150
Constante dieléctrica, 1 MHz 6.3 - ASTM D 150
Resistividad volumétrica 6.5E12 Ohm*cm ASTM D 257
Resistencia al arco 155 s ASTM D 495
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1540 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Negro
Características especiales
Estable contra el calor
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com