Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of POLYLAC PA-765A - ABS - Chi Mei Corporation

Material Data Center offers the following functions for POLYLAC PA-765A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Polylac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 48 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Contracción posterior al moldeo, paralelo 0.5 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 4.6 g/10min ASTM D 1238
Temperatura 200 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 39 MPa ISO 527
Resistencia a la tracción 29 MPa ISO 527
Módulo de flexión, 23°C 1800 MPa ISO 178
Resistencia a la flexión 56 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 23 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 10 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 22 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 10 kJ/m² ISO 180/1A
Temperatura -30 °C -
ASTM Data
Esfuerzo de fluencia a tracción 39.1 MPa ASTM D 638
Módulo de flexión 2206 MPa ASTM D 790
Resistencia a la flexión 62.5 MPa ASTM D 790
Dureza Rockwell R 101 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 235 J/m ASTM D 256
Resistencia al impacto Izod con entalla, 1/4 in 198 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 76 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 93 °C ISO 306
Temp. reblandecimiento Vicat, B 79 °C ISO 306
Coef.de expansión térmica lineal, paralelo 84.8 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-1 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 2.1 mm -
Yellow Card disponible - -
Combustibilidad 5V a espesor h 5VB class IEC 60695-11-20
Espesores de probeta 2.1 mm -
Yellow Card disponible - -
ASTM Data
Combustibilidad UL 94 V-1 - UL 94
Espesores de probeta 1.5 mm -
Estabilidad al calor @ 264 psi 76.1 °C ASTM D 648
Temperatura Vicat 92.2 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia al arco 30 s ASTM D 495
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1170 kg/m³ ISO 1183
Densidad 1170 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 85 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura del molde 40 - 70 °C -
Temperatura - zona de alimentación 180 - 210 °C -
Zona 1 190 - 220 °C -
Temperatura de boquilla 190 - 220 °C -
Contrapresión 0.5 - 1 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Ignifugante
Características especiales
Resistencia mejorada al fuego
Applicaciones
IT / Equipo de oficina, Electrica
Disponibilidad regional
Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.