Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Primefin V500/30GC - PP-GF30 - LyondellBasell Industries

Material Data Center offers the following functions for Primefin V500/30GC:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Primefin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 4 g/10min ASTM D 1238
Temperatura 230 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.003 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fluencia a tracción 79.3 MPa ASTM D 638
Alargamiento a la rotura 3 % ASTM D 638
Módulo de flexión 5516 MPa ASTM D 790
Resistencia a la flexión 86.2 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 74.7 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 264 psi 143 °C ASTM D 648
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1130 kg/m³ ASTM D 792
Características
Características
Refuerzo quimicamente acoplado, Homopolímero
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.