Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Provista™ ST - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Provista™ ST:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Provista datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastman Provista™ Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Eastman Provista™ Copolymer ST is a second-generation material that complements Eastman Provista™ by offering similar features, while providing greater toughness. Eastman Provista™ Copolymer ST is ideal in applications that place greater physical demands on the profile. Eastman Provista™ Copolymer ST is certified to NSF/ANSI Standard 51 for Food Equipment Materials.




Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.003 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 1900 MPa ASTM D 638
Esfuerzo de fluencia a tracción 47 MPa ASTM D 638
Esfuerzo de fractura a tracción 48 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 300 % ASTM D 638
Módulo de flexión 1900 MPa ASTM D 790
Resistencia a la flexión 65 MPa ASTM D 790
Dureza Rockwell R 105 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 63 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 73 °C ASTM D 648
Estabilidad al calor @ 264 psi 63 °C ASTM D 648
Temperatura Vicat 85 °C ASTM D 1525
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Brillo 143 - ASTM D 2457
Opacidad 1.3 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1250 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Extrusión de perfiles
Características especiales
Transparente
Características
High Gloss, Copolímero
Resistencia quimica
Resistencia química general
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.