Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RAVAMID® R200F T50 - PA6 - Ravago Group

Material Data Center offers the following functions for RAVAMID® R200F T50:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ravamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 45 g/10min ISO 1133
Temperatura 250 °C -
Carga 2.16 kg -
ASTM Data
Contracción posterior al moldeo, paralelo 0.012 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 75 MPa ISO 527
Resistencia a la tracción 70 MPa ISO 527
Alargamiento a rotura 55 % ISO 527
Módulo de flexión, 23°C 2800 MPa ISO 178
Resistencia a la flexión 100 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 8 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C N kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 5.5 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 4 kJ/m² ISO 180/1A
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 225 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 75 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 200 °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Glow Wire Flammability Index (GWFI) 650 °C IEC 60695-2-12
GWFI - thickness tested (1) 2 mm -
Glow Wire Ignition Temperature (GWIT) 35 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.2 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistencia dieléctrica 18 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1110 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 75 °C -
Tiempo de pre-secado 3 - 4 h -
Humedad de procesamiento ≤0.12 % -
Temperatura de la masa 240 - 270 °C -
Temperatura del molde 70 - 90 °C -
Zona 1 220 - 230 °C -
Zona 2 230 - 245 °C -
Zona 3 250 - 260 °C -
Temperatura de boquilla 250 - 260 °C -
Velocidad de giro de husillo 50 - 80 rpm -
Contrapresión 0.4 - 0.8 MPa -
Presión de mantenimiento 6 - 8 MPa -
Características
Características especiales
Alto impacto o modificado al impacto, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.