Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AMNO P20 TLD - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AMNO P20 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
PA12-P, MHLR, 12-005
Rilsamid® AMNO P20 TLD resin is a natural polyamide. This grade is plasticized and designed for injection molding.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 44 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 2.16 / * kg -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 620 / 550 MPa ISO 527
Esfuerzo de fluencia 31 / 30 MPa ISO 527
Alarg. en límite elástico 20 / 20 % ISO 527
Alarg. nominal a rotura >50 / >50 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C 9 / 14 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 3 / 3 kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 173 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 48 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 130 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 134 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 120 / * E-6/K ISO 11359-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 8 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 4 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 2010 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 595 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica - / 1E10 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E12 Ohm IEC 62631-3-2
Resistencia dieléctrica - / 26 kV/mm IEC 60243-1
Indice comparativo de linea de fuga * / 600 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.4 / * % Sim. to ISO 62
Densidad 1020 / 1020 kg/m³ ISO 1183
Funciones
Viscosidad-velocidad de cizallamiento , Rilsamid® AMNO P20 TLD, PA12, ARKEMA
Tensión de cizalla-velocidad de cizalla , Rilsamid® AMNO P20 TLD, PA12, ARKEMA
Módulo de cizallamiento dinámico-temperatura , Rilsamid® AMNO P20 TLD (Seco), PA12, ARKEMA
Esfuerzo-alargamiento , Rilsamid® AMNO P20 TLD (Seco), PA12, ARKEMA
Módulo secante-alargamiento , Rilsamid® AMNO P20 TLD (Seco), PA12, ARKEMA
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante, Plastificante
Características especiales
Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Demás información
Moldeo por inyección

Processing conditions, Injection:

- Typical melt temperature (Min / Recommended / Max) : 250°C / 270°C / 290°C.
- Mold temperature : 20 - 40°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80 - 90°C.
Resistencia a medios químicos
Acidos
Ácido acético (5% por masa) (23°C)
Solución ácido cítrico (10% por masa) (23°C)
Ácido láctico (10% por masa) (23°C)
Ácido clorhídrico (36% por masa) (23°C)
Ácido nítrico (40% por masa) (23°C)
Ácido sulfúrico (38% por masa) (23°C)
Ácido sulfúrico (5% por masa) (23°C)
Solución ácido crómico (40% por masa) (23°C)
Bases
Solución de hidróxido de sodio (35% por masa) (23°C)
Solución de hidróxido de sodio (1% por masa) (23°C)
Solución de hidróxido de amónio (10% por masa) (23°C)
Alcoholes
Metanol (23°C)
Etanol (23°C)
Hidrocarburos
N-hexano (23°C)
Tolueno (23°C)
Cetonas
Acetona (23°C)
Aceites minerales
SAE 10w40 aceite motor multigrado (23°C)
SAE 10w40 aceite motor multigrado (130°C)
SAE 80/90 aceite para engranajes hipocíclicos (130°C)
Aceite aislante (23°C)
Combustibles normales
ISO 1817 líquido 1 (60°C)
ISO 1817 líquido 2 (60°C)
ISO 1817 líquido 3 (60°C)
ISO 1817 líquido 4 (60°C)
Combustible normal sin alcohol (pref. ISO 1817 líquido C) (23°C)
Combustible normal con alcohol (pref. ISO 1817 líquido 4) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (90°C)
Combustible diesel (pref. ISO 1817 líquido F) (>90°C)
Soluciones de sal
Solución de cloruro de sodio (10% por masa) (23°C)
Solución de hipoclorito de sodio (10% por masa) (23°C)
Solución de cloruro de cinc (50% por masa) (23°C)
Otros
Acetato etílico (23°C)
Agua oxigenada (23°C)
Fluido de freno DOT no. 4 (130°C)
Glicol etilénico (50% por masa) en agua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.