Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESN BLACK P201 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESN BLACK P201 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
ISO 16396 - PA12-HlP, EGHL, C22-007

Rilsamid® AESN BLACK P201 TL resin is a black colored polyamide 12. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESN BLACK P201 TL resin falls into the PA12-PHLY category according to DIN 73378.


Main applications:
  • Air brake
  • Tubing for use in motor vehicules

Pacakaging:
This material is delivered in sealed packaging (800 kg rigid containers) ready to be procesded.

Shelf life:
Two years from date of delivery. For any use above this limit, please refer to our technical services.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 5 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 5 / * kg -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción - / 540 MPa ISO 527
Esfuerzo de fluencia - / 30 MPa ISO 527
Alarg. en límite elástico - / 22 % ISO 527
Alarg. nominal a rotura - / >50 % ISO 527
Resistencia al impacto Charpy c/entalla, -30°C - / 7 kJ/m² ISO 179/1eA
Dureza Shore D 64 / * - ISO 7619-1
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 176 / * °C ISO 11357-1/-3
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1010 / 1010 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Extrusión de perfiles, Otros tipos de extrusión
Forma de suministro
Sémola, Negro
Aditivos
Lubricante, Plastificante
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Demás información
Otros tipos de extrusión
Processing conditions:
- Typical melt temperature: (Min / Recommended / Max): 230°C / 250 °C / 270 °C
- Drying time and temperature (only necessary if containers opened for more than two hours): 4 - 6 hours at 80°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.