Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESN BLACK P210 TL - PA11-I - ARKEMA

Material Data Center offers the following functions for Rilsan® BESN BLACK P210 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
PA11-HIP, EHL, 22-007
Rilsan® BESN BLACK P210 TL resin is a polyamide 11 produced from a renewable source. This black grade is plasticized and designed for extrusion.

Rilsan® BESN BLACK P210 TL resin
falls into the PA11-PHLY category according to DIN 73378 and fulfills all specifications according to DIN 74324, ISO 7628, NFR 12632, and SAEJ844.

The biobased carbon content of Rilsan® BESN BLACK P210 TL resin is measured at 89% according to ASTM D6866.

Main applications:
  • Fluid transportation
  • Tubing for use in motor vehicle


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción - / 600 MPa ISO 527
Esfuerzo de fluencia - / 32 MPa ISO 527
Alarg. en límite elástico - / 31 % ISO 527
Alarg. nominal a rotura - / >50 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C - / 76 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C - / 10 kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 184 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 45 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 110 / * °C ISO 75-1/-2
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1030 / 1030 kg/m³ ISO 1183
Biobased content 88 % -
Características
Procesamiento y forma de entrega
Extrusión de perfiles, Otros tipos de extrusión
Forma de suministro
Sémola, Negro
Aditivos
Lubricante, Plastificante
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Certifications
Contiene recursos renovables
Disponibilidad regional
Demás información
Otros tipos de extrusión

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com