Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ 634 - PS - Trinseo

Material Data Center offers the following functions for STYRON™ 634:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 3.5 g/10min ISO 1133
Temperatura 200 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 54 MPa ISO 527
Alargamiento a rotura 2 % ISO 527
Módulo de flexión, 23°C 3500 MPa ISO 178
Dureza Rockwell R105 - ISO 2039-2
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, A 102 °C ISO 306
Temp. reblandecimiento Vicat, B 95 °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Factor de pérdidas dieléctricas, 1 MHz 6.0E-5 - ASTM D 150
Constante dieléctrica, 1 MHz 2.5 - ASTM D 150
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1050 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Certifications
Contacto con alimentos, Aprobación a contacto con alimentos 10/2011, Aprobado por el FDA 21 CFR
Applicaciones
Uso general, Empacado
Disponibilidad regional
Europa, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.