Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terluran® HI-10 - ABS - INEOS Styrolution

Material Data Center offers the following functions for Terluran® HI-10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Terluran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
High impact grade, suitable for injection moulding and extrusion.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 5.5 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Temperatura de expulsión 102 °C -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1900 MPa ISO 527
Esfuerzo de fluencia 38 MPa ISO 527
Alarg. en límite elástico 2.8 % ISO 527
Alarg. nominal a rotura 9 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 140 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 35 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 13 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 93 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 97 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 90 °C ISO 306
Coef.de expansión térmica lineal, paralelo 95 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 2.9 - IEC 62631-2-1
Constante dieléctrica, 1MHz 2.8 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 54 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 82 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E13 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 1.03 % Sim. to ISO 62
Absorción de humedad 0.21 % Sim. to ISO 62
Densidad 1030 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 250 °C ISO 294
Moldeo por inyección, temperatura del molde 60 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Funciones
Viscosidad-velocidad de cizallamiento , Terluran® HI-10, ABS, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Terluran® HI-10, ABS, INEOS Styrolution
Esfuerzo-alargamiento , Terluran® HI-10, ABS, INEOS Styrolution
Módulo secante-alargamiento , Terluran® HI-10, ABS, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 23°C, Terluran® HI-10, ABS, INEOS Styrolution
Módulo de plastodeformación-tiempo 23°C, Terluran® HI-10, ABS, INEOS Styrolution
Curva de creep 23°C, Terluran® HI-10, ABS, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 60°C, Terluran® HI-10, ABS, INEOS Styrolution
Módulo de plastodeformación-tiempo 60°C, Terluran® HI-10, ABS, INEOS Styrolution
Curva de creep 60°C, Terluran® HI-10, ABS, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Terluran® HI-10, ABS, INEOS Styrolution
Módulo a tensión-temperatura , Terluran® HI-10, ABS, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión
Forma de suministro
Sémola
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 230 - 260 °C
injection molding, Melt temperature, recommended: 250 °C
injection molding, Mold temperature, range: 30 - 60 °C
injection molding, Mold temperature, recommended: 50 °C
Otros tipos de extrusión
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Pipes, Melt temperature: 200 - 230 °C
Extrusión de perfiles
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 230 °C
Extrusión de placas
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 210 - 240 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.