Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MP200 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MP200:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastman Tritan(TM) MP200 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation copolyester can be thermoformed with a wide processing window that allows for product designs that reflect intricate detail.

Eastman Tritan MP200 copolyester is suitable for use with most forms of sterilization including radiation and ethylene oxide. It is NOT suitable for autoclave/steam sterilization. Eastman Tritan MP200 copolyester has been

formulated for use in medical film, sheet, and packaging applications.

Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Coeficiente de dilatación térmica, long. 80 E-6/K ASTM D 696
Temperatura de transición vítrea 119 °C ASTM E 1356
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.8 % ASTM D 1003
Transmitancia luminosa 93 % ASTM D 1003
Índice de refracción 1.54 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.5 % ASTM D 570
Densidad 1190 kg/m³ ASTM D 792
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
Resistencia al desgarro Trouser, parallel 10 N/mm ISO 6383-1
Resistencia al desgarro Trouser, normal 9 N/mm ISO 6383-1
Espesor de la muestra 0.254 mm -
ASTM Data
Módulo de tracción, long. 1500 MPa ASTM D 882
Módulo de tracción, normal 1400 MPa ASTM D 882
Esfuerzo de fluencia a tracción, long. 43 MPa ASTM D 882
Esfuerzo de fluencia a tracción, normal 41 MPa ASTM D 882
Esfuerzo de fractura a tracción, long. 57 MPa ASTM D 882
Esfuerzo de fractura a tracción, normal 42 MPa ASTM D 882
Alargamiento a la fluencia, long. 8 % ASTM D 882
Alargamiento a la fluencia, normal 8 % ASTM D 882
Alargamiento a la rotura, long. 114 % ASTM D 882
Alargamiento a la rotura, normal 115 % ASTM D 882
Espesor de la muestra 0.254 mm -
Características
Procesamiento y forma de entrega
Extrusion del film, Extrusión de láminas, Termoconformación
Características especiales
Estable contra el calor, Transparente, Esterilizable, Esterilización por óxido de etileno (EtO), Gamma irradiation sterilization
Características
Amorfo, Sellado en caliente, High Gloss, Copolímero
Resistencia quimica
Resistencia química general, Resistencia a la radiacion
Certifications
Grado médico, Biocompatibility ISO 10993, USP Class VI
Applicaciones
Médico, Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com