Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4300 GM42 - PBT-(GF+MF)30 - BASF

Material Data Center offers the following functions for Ultradur® B 4300 GM42:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Injection molding grade, containing a glass fiber and mineral reinforcement, for parts with good surface finish and stiffness, as well as low warpage tendency (e.g.housings).

Abbreviated designation according to ISO 1043: PBT-GF20 M10
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 17 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 7900 MPa ISO 527
Resistencia a la tracción 105 MPa ISO 527
Alargamiento a rotura 2.7 % ISO 527
Módulo de plastodeformación, 1000h 4500 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 45 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 43 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 4.5 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 223 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 195 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 220 °C ISO 75-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Combustibilidad según índice de oxigeno 21 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.8 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.8 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 12 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 150 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E13 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 300 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.4 % Sim. to ISO 62
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1550 kg/m³ ISO 1183
Propiedades específicas del materialValorUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 101 cm³/g ISO 307, 1157, 1628
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 120 °C -
Tiempo de pre-secado 4 h -
Humedad de procesamiento ≤0.04 % -
Temperatura de la masa 250 - 275 °C -
Temperatura del molde 60 - 90 °C -
Funciones
Viscosidad-velocidad de cizallamiento , Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Tensión de cizalla-velocidad de cizalla , Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento , Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo secante-alargamiento , Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 23°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 23°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 23°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 40°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 40°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 40°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 60°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 60°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 60°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 90°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 90°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 90°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 120°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 120°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 120°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Esfuerzo-alargamiento (isocrono) 160°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo de plastodeformación-tiempo 160°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Curva de creep 160°C, Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Módulo a tensión-temperatura , Ultradur® B 4300 GM42, PBT-(GF+MF)30, BASF
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Lubricante
Características especiales
Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 250 °C
injection molding, Mold temperature, range: 60 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.