Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PA - PA666 - BASF

Material Data Center offers the following functions for Ultrafuse PA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 49.5 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 196 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 49 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 65 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 135 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 172 / * °C ISO 306
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1110 / 1050 kg/m³ ISO 1183
3D DataSeco / CondUnidadesMétodo de ensayo
Other Standards[S]
Módulo de tracción, flat 2420 / 395 MPa ISO 527
Módulo de tracción, upright 2120 / 334 MPa ISO 527
Esfuerzo de tracción, flat 61.4 / 33.2 MPa ISO 527
Esfuerzo de tracción, upright 16.4 / 17.6 MPa ISO 527
Alargamiento a rotura, flat 9.6 / 143 % ISO 527
Alargamiento a rotura, upright 0.8 / 12.8 % ISO 527
Módulo de flexión, flat 2050 / 445 MPa ISO 178
Módulo de flexión, on-edge 2250 / 468 MPa ISO 178
Módulo de flexión, upright 2150 / 428 MPa ISO 178
Resistencia a la flexión, flat 77 / 17.7 MPa ISO 178
Resistencia a la flexión, on-edge 95.5 / 18.1 MPa ISO 178
Resistencia a la flexión, upright 40.2 / 17.3 MPa ISO 178
Resistencia al impacto Charpy, +23°C, flat 23 / 0 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, +23°C, on-edge 29.7 / 0 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, +23°C, upright 3.5 / 13.4 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, flat 5.6 / - kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, +23°C, on-edge 3.3 / 136 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, +23°C, upright 1.2 / 9.4 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C, flat 28 / 0 kJ/m² ISO 180/1U
Resistencia al impacto Izod, +23°C, on-edge 45.6 / 0 kJ/m² ISO 180/1U
Resistencia al impacto Izod, +23°C, upright 3.2 / 17.4 kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C, flat 5.8 / 85.4 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla, +23°C, on-edge 3.9 / 106 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla, +23°C, upright 1.7 / 10.1 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Procesamiento y forma de entrega
Additive Manufacturing
Forma de suministro
Monofilamento
Características
Estabilidad térmica
Disponibilidad regional
Norteamérica, Europa, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com