Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VANDAR® 2100UV - PBT - Celanese

Material Data Center offers the following functions for VANDAR® 2100UV:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vandar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stability, paintability, and toughness. Vandar 2100UV is available in UV stable colors.

Flammability at thickness h (1.6 mm)HB-
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 5.5 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 5 kg -
Contracción posterior al moldeo, paralelo 1.9 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.9 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1750 MPa ISO 527
Esfuerzo de fluencia 38 MPa ISO 527
Alarg. en límite elástico 4.4 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 80 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 19 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 225 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 60 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 51 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 86 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 128 °C ISO 306
Coef.de expansión térmica lineal, paralelo 130 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.6 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 70 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 200 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E14 Ohm IEC 62631-3-2
Resistencia dieléctrica 24 kV/mm IEC 60243-1
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.45 % Sim. to ISO 62
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1220 kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento , VANDAR® 2100UV, PBT, Celanese
Módulo secante-alargamiento , VANDAR® 2100UV, PBT, Celanese
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Sémola
Características especiales
Alto impacto o modificado al impacto, Estable contra rayos U.V./interperie, Estable contra el calor
Resistencia quimica
Resistencia química general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Demás información
Moldeo por inyección
To avoid hydrolytic degradation during processing, Vandar resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-30°F (-34°C) at 250°F (121°C) for 4 hours.
Rear Temperature 450-480(230-250) deg F (deg C)
Center Temperature 460-490(235-255) deg F (deg C)
Front Temperature 470-500(240-260) deg F (deg C)
Nozzle Temperature 470-510(240-265) deg F (deg C)
Melt Temperature 470-510(240-265) deg F (deg C)
Mold Temperature 100-200(40-95 deg F (deg C)
Back Pressure 0-50 psi
Screw Speed Moderate
Injection Speed Fast

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided, in particular for flame retardant grades. Up to 25% clean and dry regrind may be used.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.