Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 2000 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 2000 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Medium viscosity, unreinforced polyether ether ketone

VESTAKEEP® 2000 G is a medium viscosity, unreinforced polyether ether ketone for injection molding.

The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 2000 G are of low flammability.

VESTAKEEP® 2000 G can be processed on common injection molding machines for thermoplastics.

We recommend a melt temperature between 360°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 2000 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene inliners.

Pigmentation may affect values.

For information about processing VESTAKEEP® 2000 G, please follow the general recommendations in our brochure "VESTAKEEP® PEEK Processing Guidelines“.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 70 cm³/10min ISO 1133
Temperatura 380 °C -
Carga 5 kg -
Contracción posterior al moldeo, paralelo 1.1 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.1 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3700 MPa ISO 527
Esfuerzo de fluencia 100 MPa ISO 527
Alarg. en límite elástico 5 % ISO 527
Alarg. nominal a rotura 20 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Charpy c/entalla, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 340 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 150 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 155 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 205 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 310 °C ISO 306
Coef.de expansión térmica lineal, paralelo 60 E-6/K ISO 11359-1/-2
Yellow Card disponible - -
Combustibilidad según índice de oxigeno 38 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 2.8 - IEC 62631-2-1
Constante dieléctrica, 1MHz 2.8 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 50 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 32.6 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 200 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.5 % Sim. to ISO 62
Absorción de humedad 0.12 % Sim. to ISO 62
Densidad 1300 kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento (isocrono) 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Módulo de plastodeformación-tiempo 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Curva de creep 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Módulo a tensión-temperatura , VESTAKEEP® 2000 G, PEEK, Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Otros tipos de extrusión
Forma de suministro
Sémola
Características especiales
Estable contra el calor
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.