Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 GF30 - PEEK-GF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 GF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Glass fiber-reinforced (30%) polyether ether ketone

VESTAKEEP® 4000 GF30 is a glass fiber-re­inforced (30%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 GF30 are of low flammability.

VESTAKEEP® 4000 GF30 can be processed on common injection molding machines for thermoplastics.

We recommend a melt temperature of 380°C to 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 GF30 is supplied as cylindrical pellets in 25kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect the values.

For guidance processing of VESTAKEEP® 4000 GF30 please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines“.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 32 cm³/10min ISO 1133
Temperatura 400 °C -
Carga 21.6 kg -
Contracción posterior al moldeo, paralelo 0.3 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 11000 MPa ISO 527
Resistencia a la tracción 160 MPa ISO 527
Alargamiento a rotura 2 % ISO 527
Resistencia al impacto Charpy, +23°C 70 kJ/m² ISO 179/1eU
Type of failure C - -
Resistencia al impacto Charpy, -30°C 75 kJ/m² ISO 179/1eU
Type of failure C - -
Resistencia al impacto Charpy c/entalla, +23°C 11 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Charpy c/entalla, -30°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 340 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 312 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 335 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 335 °C ISO 306
Coef.de expansión térmica lineal, paralelo 30 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Combustibilidad según índice de oxigeno 45 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3.3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 40 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E15 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 200 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.4 % Sim. to ISO 62
Densidad 1500 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 400 °C ISO 294
Moldeo por inyección, temperatura del molde 180 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Moldeo por inyección, presión de mantenimiento 120 MPa ISO 294
Funciones
Módulo a tensión-temperatura , VESTAKEEP® 4000 GF30, PEEK-GF30, Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Sémola
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.