Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i4 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i4 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Implantable grade polyether ether ketone resin for permanent implants

VESTAKEEP® i4 G is a natural colored, high viscosity polyether ether ketone (PEEK) that is especially designed for long term implantable medical devices. This grade is often used for extrusion processing technologies.

Proven Biocompatibility of VESTAKEEP® i-Grades
The extra high purity and extended quality measures make VESTAKEEP® i-Grade materials an excellent choice for permanent implants.

For VESTAKEEP® i4 G, biocompatibility has been tested following ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i4 G complies ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.

A summary of biocompatibility test results is available upon request.

Biocompatibility tests available for i4 G


Processing of VESTAKEEP® i-Grades
VESTAKEEP® i4 G can be processed by common melt processing techniques like injection molding and extrusion.

We recommend a melt temperature between 370°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAKEEP® i4 G.

Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i4 G is supplied as cylindrical pellets in 10 kg boxes with moisture-proof polyethylene liners.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 12 cm³/10min ISO 1133
Temperatura 380 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3500 MPa ISO 527
Esfuerzo de fluencia 94 MPa ISO 527
Alarg. en límite elástico 5 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 9.1 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Charpy c/entalla, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 338 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 152 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 150 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 205 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 305 °C ISO 306
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.4 % Sim. to ISO 62
Absorción de humedad 0.12 % Sim. to ISO 62
Densidad 1300 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 380 °C ISO 294
Moldeo por inyección, temperatura del molde 180 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Sémola, Color natural
Certifications
Grado médico, Biocompatibility ISO 10993, USP Class VI
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com