Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML-GB30 - PA12-GB30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML-GB30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Microglass bead-filled (30%) PA12 resin for the injection moulding of rigid, low-warpage and dimensionally accurate mouldings

 

Biocompatibility of VESTAMID® Care ME

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation


Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 



The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY

 

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 100 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contracción posterior al moldeo, paralelo 0.6 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 / * % ISO 294-4, 2577
Densidad de fusión 1090 kg/m³ -
Conductibilidad termica de fusión 0.28 W/(m K) -
Calor especifico de la masa 2400 J/(kg K) -
Temperatura de expulsión 180 °C -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2100 / 1800 MPa ISO 527
Esfuerzo de fluencia 47 / 37 MPa ISO 527
Alarg. en límite elástico 5 / 5 % ISO 527
Alarg. nominal a rotura 20 / >50 % ISO 527
Módulo de plastodeformación, 1h * / 1600 MPa ISO 899-1
Módulo de plastodeformación, 1000h * / 1100 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy, -30°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, +23°C 4.4 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistencia al impacto Charpy c/entalla, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 55 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 150 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 155 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 130 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 130 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.1 / 5 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.5 / 4 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 310 / 600 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 230 / 370 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 / 2E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica - / 36 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / 600 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.1 / * % Sim. to ISO 62
Absorción de humedad 0.5 / * % Sim. to ISO 62
Densidad 1250 / 1260 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 250 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Moldeo por inyección, presión de mantenimiento 70 MPa ISO 294
Funciones
Viscosidad-velocidad de cizallamiento , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Tensión de cizalla-velocidad de cizalla , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Módulo de cizallamiento dinámico-temperatura , VESTAMID® Care ML-GB30 (Seco), PA12-GB30, Evonik
Esfuerzo-alargamiento , VESTAMID® Care ML-GB30 (Seco), PA12-GB30, Evonik
Módulo secante-alargamiento , VESTAMID® Care ML-GB30 (Seco), PA12-GB30, Evonik
Esfuerzo-alargamiento (isocrono) 23°C, VESTAMID® Care ML-GB30 (Cond), PA12-GB30, Evonik
Módulo de plastodeformación-tiempo 23°C, VESTAMID® Care ML-GB30 (Cond), PA12-GB30, Evonik
Curva de creep 23°C, VESTAMID® Care ML-GB30 (Cond), PA12-GB30, Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características
Baja deformación
Certifications
Grado médico, Biocompatibility ISO 10993, USP Class VI
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com