Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® D22 - PA612 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® D22:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

High-viscosity PA 612 resin

VESTAMID® D22 is a high-viscosity Polyamide 612 compound for extrusion and injection moulding of e.g. films, monofilaments (abrasive bristles).

The material based on  PA612 absorbs only small amounts of water. Components made of this material  therefore show excellent dimensional stability under changing ambient humidity.

VESTAMID® D22 is supplied as cylindrical granules in moisture-proof polyethylene containers ready for processing.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general recommendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 60 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contracción posterior al moldeo, paralelo 1.4 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.7 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2200 / 1700 MPa ISO 527
Esfuerzo de fluencia 59 / 49 MPa ISO 527
Alarg. en límite elástico 4 / 20 % ISO 527
Alarg. nominal a rotura >50 / >50 % ISO 527
Módulo de plastodeformación, 1h * / 1800 MPa ISO 899-1
Módulo de plastodeformación, 1000h * / 600 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 5 / 10 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistencia al impacto Charpy c/entalla, -30°C 7 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 215 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 60 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 140 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 180 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 130 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 120 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.8 / 5 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 / 3.7 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 230 / 650 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 290 / 550 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 / 3E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 27 / 27 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / 600 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 2.7 / * % Sim. to ISO 62
Absorción de humedad 1 / * % Sim. to ISO 62
Densidad 1060 / 1060 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 270 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Moldeo por inyección, presión de mantenimiento 70 MPa ISO 294
Funciones
Volumen especifico-temperatura (pvT) , VESTAMID® D22, PA612, Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Extrusión de perfiles, Otros tipos de extrusión
Forma de suministro
Sémola
Applicaciones
Monofilamento
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.