Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9041 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9041 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Medium-viscosity, heat and light stabilized polyamide 12 compound

VESTAMID® LX9041 BK 9.7504 s a heat stabilized and light resistant polyamide 12 compound especially developed for extrusion coating of steel tubes.
 
Due to the exceptional impact strength, abrasion resistance and good chemical resistance of PA 12 as well as the excellent adhesion between the steel and the properly applied VESTAMID® LX9041 BK 9.7504 , the corrosion resistance of steel tubes coated with VESTAMID® LX9041 black is significantly increased.

VESTAMID® LX9041 BK 9.7504 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 17 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 2.16 / * kg -
Contracción posterior al moldeo, paralelo 1.1 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.1 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1730 / 1370 MPa ISO 527
Esfuerzo de fluencia 51 / 44 MPa ISO 527
Alarg. en límite elástico 4 / 12 % ISO 527
Alarg. nominal a rotura >50 / >50 % ISO 527
Resistencia al impacto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 4 / 3.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistencia al impacto Charpy c/entalla, -30°C 4.3 / 4 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 177 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 44 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 48 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 120 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 141 / * °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.7 / 4.4 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.1 / 3.2 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 330 / 610 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 195 / 363 E-4 IEC 62631-2-1
Resistividad volumétrica específica 9.3E12 / 4.9E12 Ohm*m IEC 62631-3-1
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.3 / * % Sim. to ISO 62
Absorción de humedad 0.7 / * % Sim. to ISO 62
Densidad 1020 / - kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 240 °C ISO 294
Moldeo por inyección, temperatura del molde 60 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Características
Procesamiento y forma de entrega
Recubrimiento
Forma de suministro
Sémola, Negro
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra el calor
Características
Buenas propiedades de adhesión
Resistencia quimica
Resistencia química general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.