Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9303 BK E70288 - PA612-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9303 BK E70288:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
High-viscosity, plasticized, heat- and light-stabilized, impact-modified polyamide 612 compound for extrusion

VESTAMID® DX9303 BK E70288 is a PA 612 extrusion compound developed for the production of tubing systems with higher requirements for heat resistance.

The melting point of VESTAMID® DX9303 BK E70288 is about 35°C higher than PA 11 and PA 12 compounds, allows higher peak temperatures in use. Thereby this compound fulfills the increased demands resulting from higher temperatures in the engine compartment.

If it is intended to use VESTAMID® DX9303 BK E70288 for fuel lines, certain preconditions must be observed. The Technical Marketing assists you in finding the suitable VESTAMID® compound.
At temperatures above 100°C tubing of VESTAMID® DX9303 BK E70288 allow a higher pressure load than tubing made of PA 12 compounds with comparable flexibility.

The process temperatures should be in the range of 240-270°C.

The material absorbs only little moisture. Therefore dimensions and properties of parts are nearly unaffected through ambient conditions.


Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general recommendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 11 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contracción posterior al moldeo, paralelo 2.7 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.9 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 900 / 680 MPa ISO 527
Esfuerzo de fluencia 38 / - MPa ISO 527
Alarg. en límite elástico 30 / - % ISO 527
Alarg. nominal a rotura >50 / - % ISO 527
Resistencia al impacto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 87 / 135 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 11 / 15 kJ/m² ISO 179/1eA
Type of failure C / C(P)[C(P)] - -
Dureza Shore D 70 / * - ISO 7619-1
C(P): CAMPUS
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 211 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 20 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 60 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 142 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 159 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 150 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 120 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.7 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 2.7 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 1450 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 400 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 2E10 / 5.3E8 Ohm*m IEC 62631-3-1
Resistencia dieléctrica 39 / 34 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 2.4 / * % Sim. to ISO 62
Absorción de humedad 1 / * % Sim. to ISO 62
Densidad 1050 / - kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 250 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Características
Procesamiento y forma de entrega
Extrusión de tubería, Otros tipos de extrusión
Forma de suministro
Sémola, Negro
Aditivos
Plastificante
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra el calor
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com