Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9323 BK E70228 - PA612-I-GF35 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9323 BK E70228:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Molding compound based on nylon 612 specially suitable for plastic and rubber composites

VESTAMID® DX9323 BK E70228 is a heat-stabilized, glass fiber-reinforced and impact-modified PA 612 compound. The material contains about 35% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9323 BK E70228 is especially suitable for the production of plastic and rubber composites. 
 

Parts of VESTAMID® DX9323 BK E70228 can be directly bonded to rubber, e. g., XNBR, HNBR, AEM or FPM, without using any adhesives or adhesion promoters ("direct-bonding to rubber").

Because of its semi-crystalline morphology VESTAMID® DX9323 BK E70228 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids.
 

VESTAMID® DX9323 BK E70228 is supplied as cylindrical pellets ready for processing in moisture-proof bags.
 

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM R VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.4 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 9100 / 7400 MPa ISO 527
Resistencia al impacto Charpy, +23°C 104 / 86 kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy, -30°C 110 / 97 kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, +23°C 20 / 21 kJ/m² ISO 179/1eA
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, -30°C 15 / 14 kJ/m² ISO 179/1eA
Type of failure C / - - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 215 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 196 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 213 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 209 / * °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.8 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.6 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 610 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 320 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Indice comparativo de linea de fuga 600 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.9 / * % Sim. to ISO 62
Absorción de humedad 0.8 / * % Sim. to ISO 62
Densidad 1310 / 1330 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor
Características
Buenas propiedades de adhesión
Resistencia quimica
Resistencia química general, Resistencia a la grasa, Resistencia al aceite
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.