Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® 3013 - PBT - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® 3013:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
High viscosity polybutylene terephthalate with improved hydrolysis resistance

VESTODUR® 3013 is a high viscosity polybutylene terephthalate (PBT) resin for the extrusion, with an improved resistance to hydrolysis.

 

The resin is especially suitable for the manufacture of stiff, small-diameter tubing, e. g. for loose fiber optic buffer tubes.

 

VESTODUR® 3013 is supplied as cylindrical pellets in polyethylene packaging, ready for processing.

 

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 9 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carga 2.16 / * kg -
Contracción posterior al moldeo, paralelo 1.7 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.7 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2500 / 2450 MPa ISO 527
Esfuerzo de fluencia 57 / 57 MPa ISO 527
Alarg. en límite elástico 11 / 12 % ISO 527
Alarg. nominal a rotura >50 / >50 % ISO 527
Módulo de plastodeformación, 1h * / 2600 MPa ISO 899-1
Módulo de plastodeformación, 1000h * / 1500 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 250 / 250 kJ/m² ISO 179/1eU
Type of failure C(P)[C(P)] / C - -
Resistencia al impacto Charpy c/entalla, +23°C 5 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistencia al impacto Charpy c/entalla, -30°C 4 / 4 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistencia al impacto a tracción, +23°C 110 / - kJ/m² ISO 8256/1
Dureza Shore D 77 / * - ISO 7619-1
C(P): CAMPUS
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 223 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 45 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 55 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 150 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 180 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 110 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 110 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Combustibilidad a espesor h HB / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Combustibilidad según índice de oxigeno 23 / * % ISO 4589-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.3 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.5 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 20 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 230 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E11 / - Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E14 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 600 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 0.5 / * % Sim. to ISO 62
Absorción de humedad 0.1 / * % Sim. to ISO 62
Densidad 1310 / - kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Extrusion del film, Extrusión de tubería, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión
Forma de suministro
Sémola
Resistencia quimica
Estabilidad hidrolitica
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.