Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® GF30-FR3 NC - PBT-GF30 FR(17) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® GF30-FR3 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Glass Fiber Reinforced and Flame Retardant Polybutylene Terephthalate Compound

VESTODUR® GF30-FR3 is a glass fiber-reinforced (30% glass fiber), semi-crystalline thermoplastic compound for injection molding, based on polybutylene terephthalate (PBT), with a creamy-white color.
 
Test bars made of this compound are rated V-0, according UL94 by Underwriters Laboratories Inc., self-extinguishing and non-dripping.
 
This compound is especially suitable for parts which are subjected to high mechanical and thermal loads and must have a very good flame-resistance.

The incorporated flame retardant is non-migrating and does not contain polybrominated diphenyl ethers. The additive has no corrosive effects on metal inserts or neighboring metal parts.

Therefore, the compound is suitable for components of the electrical and electronical industry. Laser marking with high contrasts is possible.
 
The compounds are supplied as cylindrical pellets in polyethylene packaging.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM 
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 12 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.2 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.5 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 11400 MPa ISO 527
Resistencia a la tracción 130 MPa ISO 527
Alargamiento a rotura 2.2 % ISO 527
Módulo de plastodeformación, 1h 11000 MPa ISO 899-1
Módulo de plastodeformación, 1000h 8000 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 55 kJ/m² ISO 179/1eU
Type of failure C - -
Resistencia al impacto Charpy c/entalla, +23°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Dureza Shore D 84 - ISO 7619-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 223 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 45 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 216 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 223 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 213 °C ISO 306
Coef.de expansión térmica lineal, paralelo 50 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Combustibilidad según índice de oxigeno 34 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.1 - IEC 62631-2-1
Constante dieléctrica, 1MHz 4.4 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 30 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 150 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E13 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 250 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.4 % Sim. to ISO 62
Densidad 1720 kg/m³ ISO 1183
Funciones
Módulo de cizallamiento dinámico-temperatura , VESTODUR® GF30-FR3 NC, PBT-GF30 FR(17), Evonik
Volumen especifico-temperatura (pvT) , VESTODUR® GF30-FR3 NC, PBT-GF30 FR(17), Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Color natural, Blanco
Aditivos
Desmoldeante, Ignifugante
Características especiales
Resistencia mejorada al fuego, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Características
Imprimible por láser
Applicaciones
Electrica
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.