Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 41H BK0677 - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 41H BK0677:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Vydyne 41H BK0677 is general-purpose, high impact-modified, heat stabilized PA66 resin. The product offers improved resistance to thermal degradation.
41H BK0677 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 1.8 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.6 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1790 / - MPa ISO 527
Esfuerzo de fluencia 49 / - MPa ISO 527
Resistencia a la tracción 49 / - MPa ISO 527
Alargamiento a rotura 53 / - % ISO 527
Módulo de flexión, 23°C 1800 / - MPa ISO 178
Resistencia a la flexión 55 / - MPa ISO 178
Resistencia al impacto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 104 / - kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 83 / - kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 85 / - kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 41 / - kJ/m² ISO 180/1A
Temperatura -40 °C -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 262 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 56 / * °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 150 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 118 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.5 / * mm -
Combustibilidad a espesor h HB / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Ratio de combustión, FMVSS, espesor de 1mm 12 mm/min ISO 3795 (FMVSS 302)
Glow Wire Flammability Index (GWFI) 725 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 725 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Combustibilidad UL 94 HB - UL 94
Espesores de probeta 0.75 mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E8 / - Ohm*m IEC 62631-3-1
Resistencia dieléctrica 14 / - kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / - - IEC 60112
ASTM Data
Resistencia al arco 330 / - s ASTM D 495
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1070 / - kg/m³ ISO 1183
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Type of extrusion wire/cable - -
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 4 h -
Temperatura de la masa 285 - 305 °C -
Temperatura del molde 65 - 95 °C -
Zona 1 280 - 310 °C -
Zona 2 280 - 310 °C -
Zona 3 280 - 310 °C -
Temperatura de boquilla 280 - 310 °C -
Características
Procesamiento y forma de entrega
Extrusión de cable, Otros tipos de extrusión
Forma de suministro
Sémola, Negro
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor
Características
Resistencia del fundido
Resistencia quimica
Resistencia química general, Resistencia a solventes, Resistencia al aceite
Applicaciones
Automotriz, Electrica, Uso general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.