Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of WONDERLITE PC-6600 - PC - Chi Mei Corporation

Material Data Center offers the following functions for WONDERLITE PC-6600:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Wonderlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 10 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.5 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 10 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 60 MPa ISO 527
Resistencia a la tracción 70 MPa ISO 527
Módulo de flexión, 23°C 2300 MPa ISO 178
Resistencia a la flexión 90 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 60 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 15 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 60 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 15 kJ/m² ISO 180/1A
Temperatura -30 °C -
ASTM Data
Esfuerzo de fluencia a tracción 61.8 MPa ASTM D 638
Alargamiento a la rotura 100 % ASTM D 638
Módulo de flexión 2354 MPa ASTM D 790
Resistencia a la flexión 90.2 MPa ASTM D 790
Dureza Rockwell R 122 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 689 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 149 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 125 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 150 °C ISO 306
Temp. reblandecimiento Vicat, B 145 °C ISO 306
Coef.de expansión térmica lineal, paralelo 67 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 1.0 mm -
Yellow Card disponible - -
Combustibilidad 5V a espesor h 5VB class IEC 60695-11-20
Espesores de probeta 2.0 mm -
Yellow Card disponible - -
Glow Wire Flammability Index (GWFI) 930 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 264 psi 125 °C ASTM D 648
Temperatura Vicat 145 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Resistividad volumétrica específica 3.6E14 Ohm*m IEC 62631-3-1
Resistividad superficial específica 9.3E14 Ohm IEC 62631-3-2
ASTM Data
Resistencia dieléctrica, tiempo corto 1.22 kV/mm ASTM D 149
Resistividad volumétrica 1E14 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 4 h -
Temperatura del molde 70 - 120 °C -
Temperatura - zona de alimentación 230 - 300 °C -
Zona 1 250 - 320 °C -
Temperatura de boquilla 250 - 310 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Resistencia mejorada al fuego, Sin halógeno, Opaque
Applicaciones
Electrica
Disponibilidad regional
Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com