Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Carbotex K-20UVR - PC - Kotec Corporation

Material Data Center offers the following functions for Carbotex K-20UVR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Carbotex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 20 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fractura a tracción 63 MPa ASTM D 638
Alargamiento a la rotura 120 % ASTM D 638
Módulo de flexión 2160 MPa ASTM D 790
Resistencia a la flexión 85 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 740 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 V-2 - UL 94
Espesores de probeta 0.4 mm -
Estabilidad al calor @ 264 psi 131 °C ASTM D 648
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia dieléctrica, tiempo corto 20 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.009 - ASTM D 150
Constante dieléctrica, 1 MHz 2.9 - ASTM D 150
Resistividad volumétrica >1E15 Ohm*cm ASTM D 257
Resistencia al arco 110 s ASTM D 495
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 89 % ASTM D 1003
Índice de refracción 1.58 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.2 % ASTM D 570
Densidad 1200 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Estable contra rayos U.V./interperie
Características
Bajo olor
Applicaciones
Uso general
Disponibilidad regional
Norteamérica, Europa, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com