Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® 2300 GV1/30 - PBT-GF30 - Celanese

Material Data Center offers the following functions for CELANEX® 2300 GV1/30:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Chemical abbreviation according to ISO 1043-1: PBT Moulding compound ISO 7792- PBT, MGHR, 08-100N, GF30 Polybutylene terephthalate, 30 % glass fibre reinforced. Flammability UL 94 HB minimum thickness 1.2 mm. Recognition by Underwriters Laboratories, USA (UL)

Flammability @3.2mm nom. thickn.HB-
Flammability @1.6mm nom. thickn.HB-
Flammability at thickness h (1 mm)HBUL recognition (h)
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 9 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.3 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.1 % ISO 294-4, 2577
Densidad de fusión 1320 kg/m³ -
Conductibilidad termica de fusión 0.166 W/(m K) -
Calor especifico de la masa 1720 J/(kg K) -
Temperatura de expulsión 220 °C -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 10300 MPa ISO 527
Resistencia a la tracción 150 MPa ISO 527
Alargamiento a rotura 2.5 % ISO 527
Resistencia al impacto Charpy, +23°C 60 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 9.5 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 9 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 225 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 210 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 225 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 220 °C ISO 306
Coef.de expansión térmica lineal, paralelo 25 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 1.0 mm -
Yellow Card disponible - -
Combustibilidad según índice de oxigeno 20 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.4 - IEC 62631-2-1
Constante dieléctrica, 1MHz 4.3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 20 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 190 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 33 kV/mm IEC 60243-1
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.4 % Sim. to ISO 62
Absorción de humedad 0.15 % Sim. to ISO 62
Densidad 1550 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 - 140 °C -
Tiempo de pre-secado 2 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 260 - 270 °C -
Temperatura del molde 75 - 85 °C -
Funciones
Viscosidad-velocidad de cizallamiento , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Tensión de cizalla-velocidad de cizalla , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Módulo de cizallamiento dinámico-temperatura , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Esfuerzo-alargamiento , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Módulo secante-alargamiento , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Esfuerzo-alargamiento (isocrono) 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Módulo de plastodeformación-tiempo 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Curva de creep 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Esfuerzo-alargamiento (isocrono) 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Módulo de plastodeformación-tiempo 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Curva de creep 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Esfuerzo-alargamiento (isocrono) 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Módulo de plastodeformación-tiempo 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Curva de creep 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante
Características especiales
Estable contra el calor
Disponibilidad regional
Norteamérica, Europa
Demás información
Moldeo por inyección
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0,02%. The drying should be done in a dry-air dryer (dew point < -30°C) with a temperature of 120 to 140 °C and a drying time of 2 to 4 hours. In case of longer residence times in the dry-air dryer, the temperature should be reduced to 100°C.
The time between drying and processing should be kept as short as possible. The processing machine feed hopper should be closed during the processing operation.
Melt Temperature 260-270 °C
Mold Temperature *) 75-85 °C
Maximum Barrel Residence Time **) 5-10 min
Injection Speed fast
Peripheral screw speed max.0,3 m/sec
Back Pressure 10-30 bar
Injection Pressure 600-1000 bar
Holding Pressure 400-800 bar
Nozzle Design open design preferred

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided. For grades containing flame retardants, a maximum temperature of 265 °C should not be exceeded. Up to 25% clean and dry regrind may be used.

Celanese recommends only externally heated hot runner systems.

*) For moulded parts with especially high requirements to the surface quality or dimensional stability, a mold temperature of up to 110 °C can be advantageous.

**) If the cylinder temperatures are higher than the recommended maximum temperatures, the max. residence time in the barrel has to be reduced.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.