Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ EB062 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ EB062:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastman Cristal™ EB062 copolyester is a resin specifically developed for extrusion blown bottles where aesthetics

such as high clarity and gloss, coupled with design flexibility, drive demand particularly in packaging for cosmetics

and personal care. Compared to commonly used materials, Cristal EB062 runs on most standard processing

equipment. Extremely high melt strength makes the resin an excellent choice when manufacturing bottles. This

product offers improved toughness, melt strength, chemical resistance, excellent color, and clarity in thick-walled

applications. Cristal EB062 is certified to NSF/ANSI Standard 51 for Food Equipment Materials.

Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.003 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 1900 MPa ASTM D 638
Esfuerzo de fluencia a tracción 47 MPa ASTM D 638
Esfuerzo de fractura a tracción 48 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 300 % ASTM D 638
Módulo de flexión 1900 MPa ASTM D 790
Resistencia a la flexión 65 MPa ASTM D 790
Dureza Rockwell R 105 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 63 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 73 °C ASTM D 648
Estabilidad al calor @ 264 psi 63 °C ASTM D 648
Temperatura Vicat 85 °C ASTM D 1525
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Brillo 143 - ASTM D 2457
Opacidad 1.3 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1250 kg/m³ ASTM D 792
Color L 95 - CIE
Color a -0.2 - CIE
Color b 0.6 - CIE
Características
Procesamiento y forma de entrega
Otros tipos de extrusión, Moldeo por soplado
Características especiales
Alto impacto o modificado al impacto, Transparente
Características
Propiedades de barrera, High Gloss, Resistencia del fundido, Copolímero
Resistencia quimica
Resistencia química general
Certifications
Contacto con alimentos, Aprobado por el NSF 51, Food contact notification (FCN)
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.