Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DuraStar™ DS2010 - PCTA - Eastman Chemical Co.

Material Data Center offers the following functions for DuraStar™ DS2010:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Durastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Durastar™ DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2010 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2010 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing

United States Food and Drug Administration (FDA) regulations, Durastar™ DS2010 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240. This product is certified to ANSI/NSF Standard 51.




Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.004 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 47 MPa ISO 527
Alarg. en límite elástico 4 % ISO 527
Resistencia a la tracción 49 MPa ISO 527
Alargamiento a rotura 210 % ISO 527
Módulo de flexión, 23°C 1750 MPa ISO 178
Resistencia a la flexión 64 MPa ISO 178
Resistencia al impacto Izod con entalla, +23°C 29.6 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 6.3 kJ/m² ISO 180/1A
Temperatura -40 °C -
Perforación - energía, +23°C 71 J ISO 6603-2
ASTM Data
Esfuerzo de fluencia a tracción 46 MPa ASTM D 638
Esfuerzo de fractura a tracción 53.1 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 310 % ASTM D 638
Módulo de flexión 1900 MPa ASTM D 790
Dureza Rockwell 105 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 370 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 60 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 66 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 73 °C ISO 75-1/-2
ASTM Data
Combustibilidad UL 94 V-2 - UL 94
Espesores de probeta 3 mm -
Estabilidad al calor @ 66 psi 73 °C ASTM D 648
Estabilidad al calor @ 264 psi 65 °C ASTM D 648
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia dieléctrica, tiempo corto 16.6 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.015 - ASTM D 150
Constante dieléctrica, 1 MHz 2.5 - ASTM D 150
Resistividad superficial 1E17 Ohm ASTM D 257
Resistividad volumétrica 1E17 Ohm*cm ASTM D 257
Resistencia al arco 123 s ASTM D 495
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.3 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1190 kg/m³ ISO 1183
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 70 °C -
Tiempo de pre-secado 3 h -
Temperatura de la masa 250 - 290 °C -
Temperatura del molde 15 - 30 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Color natural
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Transparente
Resistencia quimica
Resistencia química general, Resistencia al aceite
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR, Aprobado por el NSF 51
Applicaciones
Empacado, Equipos deportivos
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.