Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ AN004 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ AN004:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ AN004 copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but AN004 maintains its physical properties when

exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Its processability coupled with its outstanding chemical resistance makes it well suited for thick-wall applications.




Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.004 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1800 MPa ISO 527
Esfuerzo de fluencia 47 MPa ISO 527
Alarg. en límite elástico 4 % ISO 527
Resistencia a la tracción 46 MPa ISO 527
Alargamiento a rotura 200 % ISO 527
Módulo de flexión, 23°C 1850 MPa ISO 178
Resistencia al impacto Izod con entalla, +23°C 7.8 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 4.8 kJ/m² ISO 180/1A
Temperatura -40 °C -
ASTM Data
Esfuerzo de fluencia a tracción 47 MPa ASTM D 638
Esfuerzo de fractura a tracción 51 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 320 % ASTM D 638
Módulo de flexión 2000 MPa ASTM D 790
Dureza Rockwell 103 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 80.1 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 40 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 73 °C ASTM D 648
Estabilidad al calor @ 264 psi 65 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.3 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 70 °C -
Tiempo de pre-secado 3 h -
Temperatura de la masa 230 - 280 °C -
Temperatura del molde 15 - 30 °C -
Características
Procesamiento y forma de entrega
Otros tipos de extrusión
Forma de suministro
Color natural
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Transparente
Características
Propiedades de barrera, High Gloss, Copolímero
Resistencia quimica
Resistencia química general, Resistencia al aceite
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.