Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ CN015-25 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ CN015-25:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ Renew CN015-25 Natural copolyester is a high flow product that contains a mold release to provide ease of demolding. Designed specifically for the unique requirements of luxury cosmetic packaging, our premier PCTA copolyester delivers unsurpassed color and clarity and a capability to mold thick parts with improved gate

aesthetics. Other outstanding features of Eastar™ Renew CN015-25 Natural copolyester include excellent chemical resistance, high gloss, and process enhancements such as faster drying times, faster cycle times, and lower scrap

rates. Eastar™ Renew CN015-25 Natural copolyester is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.003 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fluencia a tracción 50 MPa ASTM D 638
Esfuerzo de fractura a tracción 35 MPa ASTM D 638
Alargamiento a la fluencia 4.5 % ASTM D 638
Alargamiento a la rotura 193 % ASTM D 638
Módulo de flexión 1800 MPa ASTM D 790
Resistencia a la flexión 67 MPa ASTM D 790
Dureza Rockwell R 105 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 70 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 38 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 71 °C ASTM D 648
Estabilidad al calor @ 264 psi 63 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.6 % ASTM D 1003
Transmitancia luminosa 90 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 60 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 225 - 245 °C -
Temperatura del molde 16 - 50 °C -
Características
Procesamiento y forma de entrega
Otros tipos de extrusión
Forma de suministro
Color natural
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Transparente
Características
Sellado en caliente, High Gloss, Copolímero
Resistencia quimica
Resistencia química general
Certifications
ISCC Plus
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.