Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® HF002 - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® HF002:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
ECOZEN, conceived and developed by SK Chemicals is a bio-based, heat-resistant, and transparent bio-copolyester.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.0035 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 59 MPa ISO 527
Alarg. en límite elástico 4.3 % ISO 527
Resistencia a la tracción 34 MPa ISO 527
Alargamiento a rotura 300 % ISO 527
Módulo de flexión, 23°C 2400 MPa ISO 178
Resistencia a la flexión 79 MPa ISO 178
Resistencia al impacto Izod con entalla, +23°C 3.7 kJ/m² ISO 180/1A
Dureza Rockwell R 115 - ISO 2039-2
ASTM Data
Esfuerzo de fluencia a tracción 60 MPa ASTM D 638
Esfuerzo de fractura a tracción 42.2 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 220 % ASTM D 638
Módulo de flexión 2403 MPa ASTM D 790
Resistencia a la flexión 86.3 MPa ASTM D 790
Dureza Rockwell R 115 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 65 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 72 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 83 °C ISO 75-1/-2
ASTM Data
Estabilidad al calor @ 66 psi 79 °C ASTM D 648
Estabilidad al calor @ 264 psi 68 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 86 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1330 kg/m³ ISO 1183
Densidad 1330 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Extrusion del film, Extrusión de láminas, Moldeo por soplado
Características especiales
Estable contra el calor, Transparente
Características
Copolímero
Resistencia quimica
Resistencia química general
Certifications
Contiene recursos renovables, RoHS
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.