Any use of this information falls under the rules of our
disclaimer.
Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Contracción posterior al moldeo, paralelo |
0.2 |
% |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Esfuerzo de tracción |
88 |
MPa |
BS-2782 |
Resistencia a la flexión |
186 |
MPa |
BS-2782 |
Resistencia de compresión |
206 |
MPa |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
ASTM Data |
Combustibilidad UL 94 |
V-0 |
- |
UL 94 |
Propiedades eléctricas | Valor | Unidades | Método de ensayo |
ASTM Data |
Resistencia al arco |
180 |
s |
ASTM D 495 |
Other Standards[S] |
Resistividad volumétrica específica |
1E12 |
Ohm*m |
DIN 53482 |
Resistividad superficial específica |
1E12 |
Ohm |
DIN 53482 |
Resistencia dieléctrica |
11 |
kV/mm |
BS 2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Otras propiedades | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Absorción de agua |
0.25 |
% |
BS-2782 |
Densidad |
1800 |
kg/m³ |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Características
Procesamiento y forma de entrega
Moldeo por compresión
Forma de suministro
Compuesto de moldeo en laminas
Disponibilidad regional
Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com