Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of GADEL 2100 - PAEK - Gharda Plastics Limited

Material Data Center offers the following functions for GADEL 2100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Gadel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.01 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.011 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 3800 MPa ASTM D 638
Esfuerzo de tracción 101 MPa ASTM D 638
Alargamiento a la rotura 12 % ASTM D 638
Módulo de flexión 4200 MPa ASTM D 790
Resistencia a la flexión 165 MPa ASTM D 790
Dureza D Shore 88 - ASTM D 2240
Resistencia al impacto Izod con entalla, 1/8 in 35 J/m ASTM D 256
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 264 psi 153 °C ASTM D 648
Temperatura de fusión 344 °C ASTM D 3418
Temperatura de transición vítrea 144 °C ASTM E 1356
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1300 kg/m³ ASTM D 792
Características
Características especiales
Estable contra el calor
Resistencia quimica
Resistencia química general, Resistencia al aceite, Resistencia a la radiacion
Applicaciones
Avión y aeroespacial, Automotriz, Proceso quimico, Electrica
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.