Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Haiplen EP50 Z3 - PP - Taro Plast S.p.A.

Material Data Center offers the following functions for Haiplen EP50 Z3:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Haiplen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 8 g/10min ISO 1133
Temperatura 230 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de tracción 20 MPa ISO 527
Alargamiento a rotura >50 % ISO 527
Módulo de flexión, 23°C 850 MPa ISO 178
Dureza Shore D 63 - ISO 7619-1
ASTM Data
Resistencia al impacto Izod con entalla, 1/8 in 500 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 80 J/m ASTM D 256
Temperatura -20 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 47 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 151 °C ISO 306
Temp. reblandecimiento Vicat, B 55 °C ISO 306
ASTM Data
Combustibilidad UL 94 HB - UL 94
Espesores de probeta 3.2 mm -
Índice de oxigeno límite 21 % ASTM D 2863
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 900 kg/m³ ISO 1183
Características
Forma de suministro
Sémola
Características especiales
Estable contra rayos U.V./interperie, Estable contra el calor
Características
Bajo olor, Copolímero
Applicaciones
Automotriz, Electrica
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.