Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOS SG5009 - (ASA+PMMA) - LG Chem

Material Data Center offers the following functions for LUPOS SG5009:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupos datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 6.5 g/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Contracción posterior al moldeo, paralelo 0.7 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 6.5 g/10min ASTM D 1238
Temperatura 220 °C -
Carga 10 kg -
Contracción posterior al moldeo, paralelo 0.007 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.007 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2150 MPa ISO 527
Esfuerzo de fluencia 50 MPa ISO 527
Alarg. en límite elástico 4.3 % ISO 527
Resistencia a la tracción 43 MPa ISO 527
Alargamiento a rotura 30 % ISO 527
Módulo de flexión, 23°C 2000 MPa ISO 178
Resistencia a la flexión 70 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 5.5[1] kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 1.1[1] kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 5.4[1] kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 2.2[1] kJ/m² ISO 180/1A
Temperatura -30 °C -
Dureza Rockwell R 119 - ISO 2039-2
ASTM Data
Módulo de tracción 2284 MPa ASTM D 638
Esfuerzo de fluencia a tracción 53 MPa ASTM D 638
Esfuerzo de fractura a tracción 49 MPa ASTM D 638
Alargamiento a la fluencia 4.6 % ASTM D 638
Alargamiento a la rotura 30 % ASTM D 638
Módulo de flexión 2042 MPa ASTM D 790
Resistencia a la flexión 75.5 MPa ASTM D 790
Dureza Rockwell R 119 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 54 J/m ASTM D 256
Resistencia al impacto Izod con entalla, 1/4 in 52 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 28.5 J/m ASTM D 256
Temperatura -30 °C -
1: 4 mm
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 75 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 80 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 90 °C ISO 306
Coef.de expansión térmica lineal, paralelo 78 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 91 E-6/K ISO 11359-1/-2
ASTM Data
Coeficiente de dilatación térmica, long. 78 E-6/K ASTM D 696
Coeficiente de dilatación térmica, normal 91 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 85 °C ASTM D 648
Estabilidad al calor @ 264 psi 80 °C ASTM D 648
Temperatura Vicat 90 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E15 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E15 Ohm IEC 62631-3-2
ASTM Data
Resistencia dieléctrica, tiempo corto 23 kV/mm ASTM D 149
Resistividad superficial 1E15 Ohm ASTM D 257
Resistividad volumétrica 1E17 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1150 kg/m³ ISO 1183
Densidad 1150 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 70 - 80 °C -
Tiempo de pre-secado 3 - 4 h -
Humedad de procesamiento ≤0.01 % -
Temperatura de la masa 210 - 240 °C -
Temperatura del molde 40 - 60 °C -
Zona 1 210 - 230 °C -
Zona 2 210 - 230 °C -
Zona 3 210 - 230 °C -
Temperatura de boquilla 220 - 240 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Negro
Características especiales
Estable contra rayos U.V./interperie
Características
Resistente a rayado
Applicaciones
Automotriz, Uso general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com