Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MAGNUM™ 375 HH - ABS - Trinseo

Material Data Center offers the following functions for MAGNUM™ 375 HH:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Magnum datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 2.1 g/10min ASTM D 1238
Temperatura 230 °C -
Carga 3.8 kg -
Contracción posterior al moldeo, paralelo 0.0057 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.0056 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2330 MPa ISO 527
Esfuerzo de fluencia 47 MPa ISO 527
Alarg. en límite elástico 2.9 % ISO 527
Alargamiento a rotura 3.5 % ISO 527
Módulo de flexión, 23°C 2300 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 22 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 11 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 16 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 10 kJ/m² ISO 180/1A
Temperatura -30 °C -
ASTM Data
Módulo de tracción 2303 MPa ASTM D 638
Esfuerzo de fluencia a tracción 49 MPa ASTM D 638
Esfuerzo de fractura a tracción 8.8 MPa ASTM D 638
Alargamiento a la fluencia 3.1 % ASTM D 638
Alargamiento a la rotura 8.8 % ASTM D 638
Módulo de flexión 2406 MPa ASTM D 790
Resistencia a la flexión 76.5 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 219 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 133 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 84 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 98 °C ISO 75-1/-2
ASTM Data
Coeficiente de dilatación térmica, long. 77.4 E-6/K ASTM D 696
Coeficiente de dilatación térmica, normal 95.4 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 99.4 °C ASTM D 648
Estabilidad al calor @ 264 psi 81.7 °C ASTM D 648
Temperatura Vicat 105 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1060 kg/m³ ISO 1183
Densidad 1060 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 82 - 85 °C -
Tiempo de pre-secado 3 - 4 h -
Temperatura de la masa 243 - 271 °C -
Temperatura del molde 38 - 66 °C -
Zona 1 238 °C -
Zona 2 249 °C -
Zona 3 254 °C -
Temperatura de boquilla 249 - 254 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Estable contra el calor
Applicaciones
Automotriz
Disponibilidad regional
Norteamérica, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.