Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Makrolon® AX2477 ST - PC - Covestro Deutschland AG
Material Data Center offers the following functions for Makrolon® AX2477 ST:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Texto del producto
- MVR (300 °C/1.2 kg) 19 cm³/10 min
- low viscosity
- UV stabilized
- easy release
- developed for high-gloss surfaces with highest requirements
- for the use in combination with hard coatings
Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
ISO Data |
Indice de fluidez volumétrico, MVR |
19 |
cm³/10min |
ISO 1133 |
Temperatura |
300 |
°C |
- |
Carga |
1.2 |
kg |
- |
Índice de fluidez, MFI |
20 |
g/10min |
ISO 1133 |
Temperatura |
300 |
°C |
- |
Carga |
1.2 |
kg |
- |
Contracción posterior al moldeo, paralelo |
0.7 |
% |
ISO 294-4, 2577 |
Contracción posterior al moldeo, normal |
0.7 |
% |
ISO 294-4, 2577 |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
ISO Data |
Módulo de tracción |
2400 |
MPa |
ISO 527 |
Esfuerzo de fluencia |
66 |
MPa |
ISO 527 |
Alarg. en límite elástico |
6 |
% |
ISO 527 |
Alarg. nominal a rotura |
>50 |
% |
ISO 527 |
Módulo de flexión, 23°C |
2350 |
MPa |
ISO 178 |
Resistencia a la flexión |
98 |
MPa |
ISO 178 |
Módulo de plastodeformación, 1h |
2200 |
MPa |
ISO 899-1 |
Módulo de plastodeformación, 1000h |
1900 |
MPa |
ISO 899-1 |
Resistencia al impacto Charpy, +23°C |
N |
kJ/m² |
ISO 179/1eU |
Resistencia al impacto Charpy, -30°C |
N |
kJ/m² |
ISO 179/1eU |
Resistencia al impacto Charpy c/entalla, +23°C, 3mm |
65 |
kJ/m² |
ISO 179/1eA |
Type of failure |
P(C) |
- |
- |
Resistencia al impacto Charpy c/entalla, -30°C, 3mm |
14 |
kJ/m² |
ISO 179/1eA |
Type of failure |
C |
- |
- |
Resistencia al impacto Izod con entalla, +23°C |
75 |
kJ/m² |
ISO 180/1A |
Resistencia al impacto Izod con entalla |
12 |
kJ/m² |
ISO 180/1A |
Temperatura |
-30 |
°C |
- |
Perforación - máxima fuerza, +23°C |
5100 |
N |
ISO 6603-2 |
Perforación - máxima fuerza, -30°C |
6000 |
N |
ISO 6603-2 |
Perforación - energía, +23°C |
55 |
J |
ISO 6603-2 |
Perforación - energía, -30°C |
65 |
J |
ISO 6603-2 |
Ball indentation hardness |
116 |
MPa |
ISO 2039-1 |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
ISO Data |
Temp. de transición vítrea, 10°C/min |
143 |
°C |
ISO 11357-1/-2 |
Estabilidad al calor, 1.80 MPa |
124 |
°C |
ISO 75-1/-2 |
Estabilidad al calor, 0.45 MPa |
136 |
°C |
ISO 75-1/-2 |
Temp. reblandecimiento Vicat, B |
143 |
°C |
ISO 306 |
Coef.de expansión térmica lineal, paralelo |
65 |
E-6/K |
ISO 11359-1/-2 |
Coef.de expansión térmica lineal, normal |
65 |
E-6/K |
ISO 11359-1/-2 |
Combustibilidad a espesor h |
V-2 |
class |
IEC 60695-11-10 |
Espesores de probeta |
0.8 |
mm |
- |
Combustibilidad según índice de oxigeno |
27 |
% |
ISO 4589-1/-2 |
Glow Wire Flammability Index (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
875 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (2) |
1.5 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
930 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (3) |
3 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (2) |
1 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (3) |
1.5 |
mm |
- |
Propiedades eléctricas | Valor | Unidades | Método de ensayo |
ISO Data |
Constante dieléctrica, 100Hz |
3.1 |
- |
IEC 62631-2-1 |
Constante dieléctrica, 1MHz |
3 |
- |
IEC 62631-2-1 |
Factor de pérdidas dieléctricas, 100Hz |
5 |
E-4 |
IEC 62631-2-1 |
Factor de pérdidas dieléctricas, 1MHz |
90 |
E-4 |
IEC 62631-2-1 |
Resistividad volumétrica específica |
>1E13 |
Ohm*m |
IEC 62631-3-1 |
Resistividad superficial específica |
>1E15 |
Ohm |
IEC 62631-3-2 |
Resistencia dieléctrica |
34 |
kV/mm |
IEC 60243-1 |
Indice comparativo de linea de fuga |
250 |
- |
IEC 60112 |
Propiedades opticas | Valor | Unidades | Método de ensayo |
ISO Data |
Transmitancia luminosa |
89 |
% |
ISO 13468-1, -2 |
Otras propiedades | Valor | Unidades | Método de ensayo |
Absorción de agua |
0.3 |
% |
Sim. to ISO 62 |
Absorción de humedad |
0.12 |
% |
Sim. to ISO 62 |
Densidad |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
660 |
kg/m³ |
- |
Propiedades mecánicas (Film) | Valor | Unidades | Método de ensayo |
ISO Data |
WVTR, 23°C/85%r.h. |
15 |
g/(m²*d) |
ISO 15106-1/-2 |
Espesor de la muestra |
0.1 |
mm |
- |
Condiciones de transformación | Valor | Unidades | Método de ensayo |
ISO Data |
Moldeo por inyección, temperatura de la masa |
280 |
°C |
ISO 294 |
Moldeo por inyección, temperatura del molde |
80 |
°C |
ISO 294 |
Moldeo por inyección, velocidad de inyección |
200 |
mm/s |
ISO 294 |
Recomendación para procesamiento Moldeo por inyección | Valor | Unidades | Método de ensayo |
Temperatura de pre-secado |
120 |
°C |
- |
Tiempo de pre-secado |
2 - 3 |
h |
- |
Humedad de procesamiento |
≤0.02 |
% |
- |
Temperatura de la masa |
280 - 320 |
°C |
- |
Temperatura del molde |
80 - 120 |
°C |
- |
Zona 1 |
250 - 260 |
°C |
- |
Zona 2 |
270 - 280 |
°C |
- |
Zona 3 |
280 - 290 |
°C |
- |
Temperatura de boquilla |
290 - 300 |
°C |
- |
Contrapresión |
5 - 15 |
MPa |
- |
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Aditivos
Desmoldeante
Características especiales
Estable contra rayos U.V./interperie
Características
High Gloss
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.