Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE V2 - PP - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE V2:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 12 g/10min ASTM D 1238
Temperatura 230 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.017 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fluencia a tracción 25 MPa ASTM D 638
Alargamiento a la rotura 60 % ASTM D 638
Módulo de flexión 1600 MPa ASTM D 790
Resistencia a la flexión 45 MPa ASTM D 790
Dureza Rockwell R 100 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 33.6 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 V-2 - UL 94
Espesores de probeta 1.6 mm -
Estabilidad al calor @ 264 psi 60 °C ASTM D 648
Temperatura Vicat 100 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 940 kg/m³ ASTM D 792
Características
Características especiales
Resistencia mejorada al fuego
Características
Homopolímero
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.