Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX975 - Americas - (PPE+PA*)-MF18 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX975 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
NORYL GTX™ 975 resin is a conductive, 18% mineral reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade combines high stiffness and excellent temperature resistance with conductivity for primerless electrostatic painting. NORYL GTX975 was designed for in- or on-line painted exterior automotive trim parts such as tank flaps and corner panels.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 10 cm³/10min ISO 1133
Temperatura 280 °C -
Carga 5 kg -
ASTM Data
Índice de fluidez, MFI 15 g/10min ASTM D 1238
Temperatura 280 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 4200 MPa ISO 527
Esfuerzo de fluencia 65 MPa ISO 527
Alarg. en límite elástico 3.5 % ISO 527
Resistencia a la tracción 65 MPa ISO 527
Alargamiento a rotura 4 % ISO 527
Modulo de Flexión 4000 MPa ISO 178
Resistencia al impacto Charpy, +23°C 40 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 35 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 3 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 3 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 40 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 35 kJ/m² ISO 180/1U
Res. impacto Izod c/entalla, +23°C, 4mm 4 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 4mm 4 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 4450 MPa ASTM D 638
Esfuerzo de fluencia a tracción 69 MPa ASTM D 638
Esfuerzo de fractura a tracción 68 MPa ASTM D 638
Alargamiento a la fluencia 3.5 % ASTM D 638
Alargamiento a la rotura 4.5 % ASTM D 638
Módulo de flexión 4000 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 35 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 30 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, B 195 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 200 °C ISO 306
Coef.de expansión térmica lineal, paralelo 50 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 65 E-6/K ISO 11359-1/-2
ASTM Data
Estabilidad al calor @ 66 psi 210 °C ASTM D 648
Temperatura Vicat 215 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 3.5 % Sim. to ISO 62
Absorción de humedad 1.1 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Densidad 1250 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 100 - 110 °C -
Tiempo de pre-secado 2 - 3 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 280 - 300 °C -
Temperatura del molde 100 - 120 °C -
Temperatura - zona de alimentación 80 - 100 °C -
Zona 1 260 - 280 °C -
Zona 2 270 - 290 °C -
Zona 3 280 - 300 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Applicaciones
Automotriz
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.