Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2507F Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2507F Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Platamid® HX 2507F Pellets
Alcohol Soluble Copolyamides

Platamid® HX 2507F Alcohol Soluble Copolyamides comprises copolyamides of different structures, molecular weights and melting characteristics which are particularly well suited for coating solutions. The products offer good film forming properties, excellent abrasion resistance and good adhesion to both metallic and non-metallic surfaces. 

The main feature of all products us the ability to form stable solutions after dissolving in lower aliphatic alcohols, such as:
  • Methanol
  • Ethanol
  • Propanol / Isopropanol
  • Butanol / Isobutanol
  • or mixtures of these 

As well as in higher boiling alcohols, such as:
  • Benzyl alcohol
  • cyclohexanol
Aromatic hydrocarbons, like xylene, or SOLVESSO®, can be added at concentrations up to 20 to 30 parts by weight. These hydrocarbons do not interfere with dissolution, and improve storage stability. Solubility in conventional lacquer solvents such as ketones, esters or ethers is negligible.
All Platamid® grades are compatible in solution. This allows blending to achieve special effects. 


AVAILABLE GRADES

This grade is available:

Non-dried pellets („F“) with a maximum residual moisture content of ≤ 1.8 %

PACKAGING

In 25 kg paper bags with aluminium foil / polyethylene liners on 1000 kg pallets

SHELF LIFE

Two years from the date of delivery. For any use above this limit, please refer to our technical services.



Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 0.6 / * cm³/10min ISO 1133
Temperatura 190 / * °C -
Carga 2.16 / * kg -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 155 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 115 / * °C ISO 11357-1/-2
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 4.5 / * % Sim. to ISO 62
Densidad 992 / 992 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Extrusion del film, Recubrimiento
Forma de suministro
Sémola
Características
Resina de mezcla, Buenas propiedades de adhesión, Copolímero
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.