Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Índice de fluidez, MFI |
12 |
g/10min |
DIN 53735 |
Temperatura |
220 |
°C |
- |
Carga |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
ISO Data |
Resistencia al impacto Charpy c/entalla, +23°C |
10 |
kJ/m² |
ISO 179/1eA |
Resistencia al impacto Izod con entalla, +23°C |
17 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
Módulo de tracción |
2400 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Temp. reblandecimiento Vicat, B |
95 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Otras propiedades | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Densidad |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Características
Forma de suministro
Negro
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.