Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® BF40 L - PA6 - Nurel S.A.

Material Data Center offers the following functions for Promyde® BF40 L:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 220 °C ISO 11357-1/-3
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 5[1] % ASTM D 1003
1: Chill roll temperature 90ºC
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 9 % Sim. to ISO 62
Absorción de humedad 3 % Sim. to ISO 62
Densidad 1130 kg/m³ ISO 1183
Moisture Content 0.1 % -
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
Tensión a fluencia, paralelo 34 MPa ISO 527-3
Resistencia a la tracción, paralelo 96 MPa ISO 527-3
Alargamiento máximo, paralelo 350 % ISO 527-3
Resistencia al desgarro Trouser, parallel 25 N/mm ISO 6383-1
Coeficiente dinámico de fricción 0.25 - ISO 8295
WVTR, 23°C/85%r.h. 15 g/(m²*d) ISO 15106-1/-2
Prop. de transm. de oxígeno, 23°C/0%r.h. 25 cm³/(m²*d*bar) ISO 15105-1/-2
Prop. de transm. de oxígeno, 23°C/85%r.h. 40 cm³/(m²*d*bar) ISO 15105-1/-2
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 75 - 80 °C -
Temperatura - zona de alimentación 230 - 240 °C -
Zona 1 250 - 265 °C -
Zona 2 255 - 265 °C -
Temperatura de boquilla 255 - 265 °C -
Características
Procesamiento y forma de entrega
Extrusión de película soplada, Extrusion del film, Otros tipos de extrusión, Termoconformación
Aditivos
Lubricante
Características
Propiedades de barrera
Resistencia quimica
Resistencia química general
Certifications
Contacto con alimentos
Applicaciones
Empacado
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.