Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P302 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P302 TL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
ISO 16396 - PA12-HIP, EGHL, C22-004

Rilsamid® AESNO P302 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P302 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Air brake. 
Tubing for use in motor vehicles

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 13 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 5 / * kg -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 475 / 430 MPa ISO 527
Esfuerzo de fluencia 28 / 24 MPa ISO 527
Alarg. en límite elástico 24 / 24 % ISO 527
Alarg. nominal a rotura >50 / >50 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C 46 / - kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 4 / 6 kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 174 / * °C ISO 11357-1/-3
Coef.de expansión térmica lineal, paralelo 150 / * E-6/K ISO 11359-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E12 / 1E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 7E13 Ohm IEC 62631-3-2
Resistencia dieléctrica 41 / 41 kV/mm IEC 60243-1
Indice comparativo de linea de fuga * / 600 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.2 / * % Sim. to ISO 62
Densidad 1030 / 1030 kg/m³ ISO 1183
Funciones
Viscosidad-velocidad de cizallamiento , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Tensión de cizalla-velocidad de cizalla , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Módulo de cizallamiento dinámico-temperatura , Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
Esfuerzo-alargamiento , Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
Módulo secante-alargamiento , Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
Esfuerzo-alargamiento (isocrono) 23°C, Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
Módulo de plastodeformación-tiempo 23°C, Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
Curva de creep 23°C, Rilsamid® AESNO P302 TL (Seco), PA12-I, ARKEMA
LTHA-Alargamiento a rotura  2mm, Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Otros tipos de extrusión
Forma de suministro
Sémola
Aditivos
Lubricante, Plastificante
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Demás información
Extrusión de perfiles

Processing conditions, Extrusion :

- Typical melt temperature (Min / Recommended / Max) : 200°C / 220°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.

Resistencia a medios químicos
Acidos
Ácido acético (5% por masa) (23°C)
Solución ácido cítrico (10% por masa) (23°C)
Ácido láctico (10% por masa) (23°C)
Ácido clorhídrico (36% por masa) (23°C)
Ácido nítrico (40% por masa) (23°C)
Ácido sulfúrico (38% por masa) (23°C)
Ácido sulfúrico (5% por masa) (23°C)
Solución ácido crómico (40% por masa) (23°C)
Bases
Solución de hidróxido de sodio (35% por masa) (23°C)
Solución de hidróxido de sodio (1% por masa) (23°C)
Solución de hidróxido de amónio (10% por masa) (23°C)
Alcoholes
Metanol (23°C)
Etanol (23°C)
Hidrocarburos
N-hexano (23°C)
Tolueno (23°C)
Cetonas
Acetona (23°C)
Aceites minerales
SAE 10w40 aceite motor multigrado (23°C)
SAE 10w40 aceite motor multigrado (130°C)
SAE 80/90 aceite para engranajes hipocíclicos (130°C)
Aceite aislante (23°C)
Combustibles normales
ISO 1817 líquido 1 (60°C)
ISO 1817 líquido 2 (60°C)
ISO 1817 líquido 3 (60°C)
ISO 1817 líquido 4 (60°C)
Combustible normal sin alcohol (pref. ISO 1817 líquido C) (23°C)
Combustible normal con alcohol (pref. ISO 1817 líquido 4) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (90°C)
Combustible diesel (pref. ISO 1817 líquido F) (>90°C)
Soluciones de sal
Solución de cloruro de sodio (10% por masa) (23°C)
Solución de hipoclorito de sodio (10% por masa) (23°C)
Solución de cloruro de cinc (50% por masa) (23°C)
Otros
Acetato etílico (23°C)
Agua oxigenada (23°C)
Fluido de freno DOT no. 4 (130°C)
Glicol etilénico (50% por masa) en agua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com